Towards a new stress corrosion test applicable to prestressing steels
Towards a new stress corrosion test applicable to prestressing steels
RAHARINAIVO ; GAILLET
Type de document
COMMUNICATION ORALE SANS ACTES (COM)
Langue
anglais
Auteur
RAHARINAIVO ; GAILLET
Résumé / Abstract